Shanghai Gengyun Industrial Co., Ltd
Recycled Halogen-Free Zero Halogen Flame Retardant Cable Material/Tpugranules Elastomer TPU Material
The recycled thermoplastic polyurethane elastomer tpu material is a kind of environmental friendly inflaming retarding thermoplastic elastomer cable material. It has excellent mechanical performance and processing performance,and fine flame retardant property.It meets IEC-60332-1-1 standard. TPU material is widely used in metro,ships,program-controlled machine room of power cable,optical cable,signal cable and various data transmission cable.
Feature
- Good electrical insulation;
- Has flame retardant;
- Low acetaldehyd content, good color,;
- Stable viscosity and low heavy metal content;
- TPU Elastomer has higher strength;
- Better barrier, transparency;
- Good machining performance;
- With excellent barrier performance;
- Elastomer tpu material can meet the requirements of hot filling beverage filling below 90ºC. And the bottle deformation rate is low;
- Through modified TPU, the flame retardant level can reach VO level, no halogen low smoke flame retardant;
- With flexible and high strength characteristics, hydrolysis and aging resistance;
- Thermoplastic extrusion processing, simple process;
- The surface fog surface, will not produce precipitation, strong stability;
- Thermoplastic polyurethane meet the environmental protection requirements of RoHs and REACH;
Application
The oil resistance, water resistance, and chemical resistance of the TPU sheath make it an ideal choice for cables used in marine applications.
Outdoor optical cable sheath materials, such as pipeline optical cables, direct buried optical cables, underwater optical cables, etc;
Plastic TPU Sheaths for industrial machinery and equipment;
Processing
The following temperature profile of extruder is recommended:
Zone | Zone1 | Zone2 | Zone3 | Zone4 | Zone5 | Head | Die | |
ºC Temperature |
130 | 140 | 145 | 150 | 155 | 160 | 160 |
Properties of TPU Thermoplastic Polyurethane
NO. | ltem | Unit | Typical value | Test method | ||
T-TP004-E-8505 | T-TP004-E-8605 | |||||
1 | Density | g/cm² | 1.45 | 1.40 | GB1033 | |
2 | Tensile Strength | MPa | 12 | 13 | GB1040 | |
3 | Elongation at Break | 200 | 230 | |||
4 | Thermal Aging Property | C x day | 100×7 | 100×7 | GB/T2951.7 | |
4.1 | Variation on Tensile Strength | % | -9 | -8 | ||
4.2 | Variation on Elongation | % | -12 | -12 | ||
5 | 90ºCx 4h Hot Deformatior |
% | 18 | 19 | GB8815 | |
6 | Brittle Temperature at -40ºC | pc | 0 | 0 | GB5470 | |
7 | Volume Resistivity at 20ºC | Q.m | 2.8×10 | 2.8×10 | GB1410 | |
8 | Dielectric Strength | MV/m | 27 | 27 | GB1408 | |
9 | Smoke Density |
Flaming | — | 58 | 58 | ASTM E 662 |
No flaming | — | 220 | 210 | |||
10 | Oxygen Index | % | 29 | 30 | GB2406 | |
11 | Content of Halogen Acid | IEC60754-2 | ||||
11.1 | PH Value | — | 5.8 | 5.8 | ||
11.2 | Electrical Conductivity | μ s/mm | 2.0 | 2.0 | ||
12 | Toxicity Index | — | 1.4 | 1.4 | NES 713 |